Cart 0
Superalloys
Click to zoom

Share this book

Superalloys : Analysis and Control of Failure Process

Book Details

Format Hardback or Cased Book
ISBN-10 1138094358
ISBN-13 9781138094352
Publisher Taylor & Francis Ltd
Imprint CRC Press
Country of Manufacture GB
Country of Publication GB
Publication Date Jan 16th, 2019
Print length 290 Pages
Weight 624 grams
Dimensions 16.40 x 23.90 x 2.40 cms

AI Summary

Ksh 36,000.00
Werezi Extended Catalogue 0 in stock

Delivery Location

Delivery fee: Select location

Secure
Quality
Fast
Superalloys have a wide variety of applications, especially as the parts of gas turbines for aircraft and electric power stations. This book presents the results of the scientific studies on the three types of superalloys (Ni3Al-based, Iron-based, and Co3(Al,W)-based) including industrial gas turbine blades after accident.

Superalloys form a class of the structural materials for high-temperature applications. Nickel superalloys are extensively used in the high-temperature components of gas turbines due to their excellent creep, fatigue, and corrosion resistance at elevated temperatures. These materials are considered paramagnetic in the range of working temperatures. This book presents the features of the ternary phase diagrams Ni-Al-X (X = {Co, Fe, Nb, Ti, Cr}), effects of the alloying on the long-range order and mechanical properties of the Ni3 Al-based alloys.

Description of the strain-induced ferromagnetism in the Ni3Al-based alloys and magnetic control of the failure of gas turbine blades are also included. A separate section is devoted to the analysis of the vibration process and strength change in the single-crystal gas turbine blades.

This book includes the review of the new intermetallic cobalt superalloys. The structure, crystal lattice parameters, orientation relationships between phases, mechanical and magnetic properties of the Co3(Al,W)-based alloys are described.

Non-destructive magnetic point control of the martensite content in low-magnetic austenitic alloys is a new method for detection of the local sites with internal stresses. This method is useful for the detection of the residual stress in the critical parts of industrial products.

This book may be useful for specialists in material science, first-year postgraduate students taking a class in material science and engineering, and engineers developing new alloys for the gas turbine technology.


Get Superalloys by at the best price and quality guaranteed only at Werezi Africa's largest book ecommerce store. The book was published by Taylor & Francis Ltd and it has pages.

Discover books you might love based on this title.

Shopping Cart

Africa largest book store

Sub Total:
Ebooks

Digital Library
Coming Soon

Our digital collection is currently being curated to ensure the best possible reading experience on Werezi. We'll be launching our Ebooks platform shortly.